(a)
(a)
(b)
Figure 8. (a) An example of sustained load cracking (SLC) in Ti-6Al-4V where macroscopic growth (>1 mm) was observed at temperatures below 273K (0°C) [28]. (b) SLC observed in this study (at room temperature) was microscopic in that the crack propagated less than 100 mm before eventual arrest.